>     My sister bought necklaces for her bridesmaids that were made from
>     various beads and a type of wire said to be "gunmetal" by the lady
>     who made and sold the necklaces to her. 

    Were these on gunmetal CHAIN or wire? To the best of my knowledge
    "gunmetal" is a dark plating applied to brass chain. I have seen it
    on ready made chains. Rings and Things in Spokane Washington used to
    carry it in footage chain. When it was really "in" you saw it on lots
    of inexpensive austrian crystal necklaces. 

    The craft wire you mentioned I have seen too: it is usually a copper
    core with a coating almost like a colored plating; you can get
    aluminum wire too that has been anodized and colored. I have played
    around with these and the coating cannot take much handling, plier
    bending, etc. If what you do involves something complex it will
    chip/nick/wear off quickly. Plus the core color will show at the
    ends. Annealing or polishing is not possible. 

Lin Lahlum


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project