>>    salt will eat right through them). 

>     curious as to whether repeatedly getting jewelry wet in the salt
>     water would have any effect over the long term? 

    Although an experiment would give greater answers, thinking about it
    I can simply advise rising the jewellery off when you come out of the
    sea (most likely pat dry too, but is not part of the salt eating
    soldering joint problem), for if you let the sea water evaporate and
    a fine layer of salt to form then leave it for a time and repeat you
    will most assuredly see a weakening and eventual failure of your
    joints. Most people are likewise cautious of swimming pools and the
    chlorine involved. Just take care of your jewellery and all should be
    fine. Personally I would rinse coming out of the ocean, or as soon as
    convenient. 

Hope that helps dissuade your fears.

Kindest,
K. David Woolley
david.woolley AT unb.ca


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project