========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Once again, the discussion of what is STERLING SILVER has appeared in one of the metal clay groups. Several writers there insist that Sterling Silver is 92.5 Fine Silver and the rest can be any other metal. One person posted a law that states the above. So, my question is: Does the above definition apply to Hollow Ware rather than Jewelry grade Sterling Silver? I seem to remember reading a long discussion regarding this issue. I know that in Europe the use of Nickle is not allowed in Sterling. But what about in the USA? Some manufacturers insist that their product is "nickle compliant." What about sheet and wire products; are they also "nickle compliant?" Along with that, let me also ask: Is Argentinium Silver called Sterling Silver? When selling items made Argentinium, can they be stamped .925? or Sterling? If not, how would one mark items made from the non-tarnishing alloy? Thanks in advance! ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project