Re: [Orchid] Which wax does one use?  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: LEESSILVER
Date: Sat Jan 14 19:37:37 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    The types of tools you will need to carve wax depend on what you
    want to create. 

    Files and a foredom with several types of burrs will come in handy
    if you plan on carving wax. Carving waxes are non sticky, non
    flexible and may be worked with files, sandpaper, pocket knives,
    dental tools, any type of scraping tools and burrs mounted in a cable
    driven handpiece. The biggest problem when working with carving wax
    is breakage of the model. As with all wax models you can wax weld
    errors and breakage. 

    Wax build up, the layering of hot wax on top of previously layered
    on wax and construction, building a model with various cut pieces of
    waxes, will require different tools. 

    Models can be built using a combination of all the types on
    construction. 

    Construction models are most difficult to work with because the
    waxes normally used are soft and very flexible. When working on a
    construction model care must be excised to prevent reshaping it every
    time you pick it up. 

    I have found that dental tools are a great help in carving wax. I
    modify some of them to suit the job I want to do. 

    Check out: http://www.ganoksin.com/borisat/nenam/dental-tools.htm 

    Be happy to send, off line, pictures of the various types of wax
    model making. Oh boy!!!! Here we go again. I see a paper illustrating
    the various types of constructions. Tomorrow I will break out my
    camera and lap top and start the new project for what its worth. 

Lee Epperson

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project