========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You don't mention if you are working with Sterling Silver or Fine Silver. Fine silver is easier to granulate with. I have never used the copper coating with silver granules, only with gold, and that is a step which you can eliminate. Hide glue is still sold in some old fashioned hardware stores, or suppliers for woodworkers. It is a brownish color, and is a thick, slow running substance. If you can find it in it's sluggishly liquid form, you can use it directly from the bottle. I've never run into a problem with additives. The mixture to use for the 'granule holding' process is: approximately 10 drops water, one or two drops hide glue, and about 4 drops of liquid flux, using a small eye dropper. Remember to heat the piece with the hide glue on it in slow stages, and have it set in the kiln before you heat it enough so the hide glue dissolves away. At that point the granules are loose and will fall off or roam around if you move the piece. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project