========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, Spider, > Is the rust issue so insurmountable? I guess this isn't the popular notion, but we used regular steel shot for many years where I teach, without drying it. There was never any problem except when the solution was allowed to get too low. As long as the shot was covered with (soapy) water, no rust. On the other hand, I tried that magnet trick just once. What a fiasco! It really didn't work. I ended up sorting by hand, for what seemed like hours. No matter how many jump rings you make, I really think it's gotta be more efficient to string them! If you try it, let me know how it goes, Noel ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project