    I've been told that I should stick with stainless shot because the
    mild steel shot is just too hard to maintain. But it would be SO
    convenient to be able to separate my batch with a magnet, and the
    stainless shot is ba-aa-arely magnetic. I could get a really strong
    magnet, or I could get mild steel shot. 

    Is the rust issue so insurmountable? I always dry my batch of jump
    rings & shot completely in a cool oven, so the shot wouldn't be
    sitting around for days being damp. And if I do get a bit of rust on
    the shot, will it contaminate my sterling jump rings beyond easy
    repair? 

    And you needn't suggest running a wire through the coils to keep the
    jump rings grouped up. I make enough jump rings that this (very
    clever) trick isn't practical for me. 

    Help me Orchid! You're my only hope! 

    -Spider (going a little bit loopy after an extremely productive day)

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project