    A slow response to this question.. The silver brazing alloys that
    contain copper start to lose the silver tint as the copper content
    increases. There are many alloys that have a brass tint that do not
    contain cadmium. I have used mostly easyflow 35 - but the cadmium
    containing one for about 40 years on and off. I don't try to breath
    in the vapours along with flourides from the active fluxes. Never
    smoked though- still kicking. 

    If you look through the modern listings you will find many cadmium
    free alloys and some cadmium containing. Some of the suppliers have
    discontinued making selling cadmium containing versions totally.. It
    won't be hard to find brass colored ones. The degree of color
    matching acceptibility is up to you see: 

    http://www.jwharris.com/jwprod/hisilverbrazealloys/ 

    http://www.brazing.com/products/Braze_silver/ 

    http://tinyurl.com/dk6wc

    http://www.lucas-milhaupt.com/ part of Handy and Harmon 

    Joining with parent metal as the filler material is really welding --
    you probably don't want to do this since you don't wish to melt the
    parts just the filler. 

    You should be able to get close to what you want. Download the
    reference guides! 

    A harder job is matching copper color. with a brazing alloy. In this
    content only gilding metal ( 95% copper 5%zinc) comes close. in a
    reasonably available material.. 

    You will find a few alloys that contain that contain a small
    percentage of nickel- these are not jewelry fabrication materials but
    are intended for brazing stainless steel where they wet the surface a
    bit better. Allergy conditions are an individual issue. 

jesse


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project