>     Here's a photo so anyone can see the problem.
>     http://www.ganoksin.com/ftp/bb.jpg I wonder if throwing it in a
>     tumbler with steel shot would take the black stuff off but still
>     preserve (or enhance) the polish? Another piece of equipment I've
>     been meaning to buy... 

    I boil work in water with SOAP, not detergent (detergent can leave a
    film on diamonds) In a small dish, I use enammell one, dissolve hand
    soap in hot water untill it is cloudy, boil and then add about half
    a teaspoon of ammonia, clean work with a tooth brush, scrubbing and
    using a jabbing action from all angles. I always have a pot of this
    and clean just about every thing thats safe to go in hot water and
    ammonia. You need to use it hot to help soften polish. 

    It sets when cold because there is so much saop in solution. 

    You will have to add ammonia each time you use it because it
    evapourates. 

    This is an old recipe always works really well. 

    Ammonia degreases, is a STRONG alkali, opposite to acid, can be
    equally dangerous especially industrial stuff. I use household
    ammonia, not half as strong, in a well ventilated room. Always use
    hand cream afterwards. 

Mary.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project