>     A process you might want to look for is called sublimation. The
>     metal pieces will have a special coating on them and you will have
>     to print your image on a special paper and apply to the metal with
>     a heat press. Good luck... 

    The special coating is polyester in liquid form, you usually dip or
    spraycoat the item. 

    You'll need a special paper but also a special ink for your printer.
    To top it off, I always recommend a second printer for the
    sublimation ink because it will create less problems and maintain a
    good economy. (Switching cartridges entails intensive cleaning of
    the heads.) 

    As for a heat press - in the T-shirt business it's callerd
    transferpress (at least in Europe) - it should not press hard like
    you would with textiles but heat evenly which could become a problem
    if you aim to do irregular forms. In a production situation there
    are ways to solve this. 

    Please ask if you have any questions. 

michaela

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project