Peter

    The Mouth Blow Pipe ( no torch or bottled gases) with a Lamp &
    charcoal is still used by 75% of all Indian & Pakistani jewelers for
    their soldering work. The only difference is that most of these
    Jewelers are working with at least 18K and Fine silver. 

    Although they have the Foot Pump and a Pressurized Kerosene setup
    with primitive blow pipes & limited tips. Yet when it comes to
    precision fine soldering work they would rather use the mouth blow
    torch. 

    I sell these Brass pipes and there are a few dealers that still buy
    these for the Art Classes. 

    The torch that you are talking with a provision of adding forced air
    by mouth was very common in Europe and in Japan. When I started in
    this business (1974) almost all of the Foreign tool suppliers showed
    at least one or more in their catalog. 

    Similar to a cutting torch but one where you will not have the
    tremendous pressure but can actually regulate by mouth. 

Regards Kenneth Singh


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project