Kimberly and All,

>     Would your method possibly work in my situation? If you were
>     cleaning a clasp on a strand of pearls in this way, would it
>     damage the silk the pearls are knotted on or do you just avoid
>     getting the silk wet.

    The recipe is one tbsp Calgon water softener, powder or liquid, one
    tbsp salt, two cups water in a glass or plastic container. Do not
    use Calgon product that has oil in it. We use cold water. Put the
    aluminum foil on the bottom of the container, put the tarnished item
    on the foil, remove, rinse, and dry. Do not leave the foil in the
    solution, as the foil will disintigrate over a day or two. As far as
    silk and pearls, it has not done harm to any pearl or gem materials
    that have been strung. Do not let it soak, just in and out.. My wife,
    from experience over the years, does not use silk as it stretches too
    much. Wet silk would probably stretch easier, so if it is real silk,
    lay them flat to dry.

Richard Hart

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project