========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== My experiences with aluminum are more along the lines of structure - machine shop and the like - There is a compelling link between ingesting aluminum (pots and pans) and alzheimer's disease. Just something to keep in mind. I don't recall the number, but most of the aluminum you'll find is pure (99.9) aluminum - that's what most of the aluminum things that are around you, especially extruded things, are made of. Soda cans, for instance. I use onlinemetals.com for all my industrial metals - decent selection, good prices. You can get metals quite a bit cheaper on ebay, but it's harder to get just what you want. It can be soldered with aluminum flux, but it's quite difficult. Others may offer better solutions, but the only coatings I know of that work involve anodizing, which is very involved. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project