    Here is a post from Metal Clay Gallery yahoo list that may shed some
    light on the recent question about the metal clay turning brassy. 

    Elaine 

          I have been using dry casting investment (powder) as a support
          for odd shaped/hollow objects, I use a dust mask. It works
          great but I have noticed that the items develop a golden/brassy
          tarnish, at the contact points with investment, within 10
          minutes in my tumbler. Scrubbing with a wire brush doesn't
          remove it. This tarnish only comes off with (yikes)Tarnex! I've
          tried a good long soak in strong hot pickle and it just doesn't
          work as well. After the 2 minute Tarnex dip I rinse it in water
          then neutralize it in hot baking soda and water. The pieces
          tumble up beautifully after the dip. I <snip> Vicki 

Elaine Luther
Metalsmith, Certified PMC Instructor
http://www.CreativeTextureTools.com (TM)
Hard to Find Tools for Metal Clay

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project