From: Karen Christians Date: Thu Dec 29 05:47:00 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Leona, You also want to watch temperature in which you pickle. You never want to toss your freshly soldered piece directly into the hot pickle as the temperature change and the acid will begin burrowing little pits. Let the joint cool a bit and then quench in water first, then pickle. The small amount of zinc in solders burns away each time you heat it back up. Your joint actually does become harder and more brittle, although I am not sure it is the pickle that does this. Different companies make different solder alloys. My personal choice? Hoover and Strong. They make an excellent solder. For gold I would go with Otto Frei. Theirs works very well. -k Karen Christians M E T A L W E R X 50 Guinan St. Waltham, MA 02451 Ph. 781/891-3854 Fax 3857 http://www.metalwerx.com/ Jewelry/Metalarts School & Cooperative Studio ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project