Hi Mr Hart:

>     Retail store experience...... we use the aluminum foil, Calgon,
>     salt, solution for cleaning sterling silver with every type of
>     stone you can think of with absolutely not one piece suffering any
>     detectable damage. Hundreds of customers have been given the
>     recipe and no reports of damage over the years. If an object can be
>     put in water with no damage, this solution would not damage
>     anything I can think of. 

    I have been making an earring from weaving together tiny (very tiny)
    sterling silver beads on nylon or silk beading thread. The earrings
    are very nice (if I can be so bold) but, I have had no way to clean
    them if they get tarnished. 

    Would your method possibly work in my situation? If you were
    cleaning a clasp on a strand of pearls in this way, would it damage
    the silk the pearls are knotted on or do you just avoid getting the
    silk wet?( I know you said in the above post that it doesn't damage
    anything that you can think of, but I just wanted to double check. I
    can be annoying in that way). If it is not a trade secret, would you
    be willing to share the ratio of the ingredients in the solution? 

    Thank you and I always look forward to reading your posts. I have
    learned a lot from them. 

Best Regards,
Kim Starbard
Cove Beads

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project