Hi, Lori,

>     Put the stone in and when I go to set it, I have to much bezel
>     wire and the corner split.

    If your bezel split when you tried to close it, it may be that the
    bezel is higher than needed. If it is only just as high as it needs
    to be to hold the stone in, you shouldn't have to push it very far
    before it contacts the stone. 

    Second, try pushing on the corners first. It is difficult to push
    the corners down to the stone, but it is much harder to do it after
    the sides are down.. If you close the corners first, then move on to
    work on the sides, you should get a neater look. 

    If they still come apart, there is probably a problem with the
    construction of the bezel in the first place. It sounds as though
    you are constructing the bezel from four pieces with seams at the
    corners. If this is the case, those corners are going to be *very*
    stiff. You might make your bezel out of one piece, with the seam in
    the center of a side. If you are using thick material, you will need
    to cut/score along the bend line halfway through or more with a
    separating disc or one corner of a square file to get a neat, sharp
    bend. 

    If none of this sounds right, you may need to give us more
    information about what you're doing (I don't have the book you
    mentioned). 

Noel

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project