From: ATG Date: Mon Dec 26 06:07:00 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Christine, I work in Silver metal clay and although I can't tell you why it turned brassy, I can suggest a way to get the shine back. Why don't you try using a Dremel polishing wheel with red rouge to gently buff it up? I use this on my pieces and it makes them look just brilliant, with very shiny mirror finish. If this doesn't work, let me know. I have some other suggestions. However, I would not use harsh chemicals on it, so let me know if you need more suggestions. Remember it is pure silver (.999) and may more easily combine chemically with other substances (like ammonia) because of this. Hope this helps! Laura ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project