From: Noel Date: Sun Dec 25 02:02:19 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, John, Merry Christmas! Your reply about the "fresh" hydrogen gas made me wonder-- why do the hydrogen atoms hook up with the sulphides instead of just pairing with their mates (other naked hydrogen atoms)? Also, Jim said sodium carbonate bubbled more than bicarb did. Is more hydrogen liberated from the carb than the bicarb, making it more effective? --Noel (who used to kinda understand chemistry, an awful long time ago, and is still curious) ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project