    Believe it or not, you can use a little regular toothpaste on a soft
    cloth to clean ivory. Sort of like you would use furniture paste on
    wood. Rub onto the spot. Buff off by hand. If the spotting is oil
    based, or from a man made product, chances are it will not come off.
    If the beads are old, then the discoloration might be the natural
    variations of the ivory. If I could see the "spots" I would have a
    better idea, but the toothpaste works well for cleaning ivory and
    doesn't harm it. If you want to know how I figured this one out, I
    am a handcarver of fossilized ivory. The Inuits that I buy tusks from
    told me this one. 

    Good luck, 

    Lisa, (Fabricating for the first time in white gold. Boy do I not
    like this stuff! But on a good note, I did plant a strawberry tree in
    the yard yesterday.) Topanga, CA USA

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project