    Yes I know about dirilyte. It was a flatware option mid 20th
    century. I had a set of flatware with the salt and pepper shakers
    that you have. The material was a rosy bronze, and originally was
    coated to retard tarnish. I got rid of it when it became obvious that
    it couldn't go in the dishwasher. Who want to hand was flatware?

    Your problem is the salt has corroded the interior. First I'd try to
    shake all the salt out, and then soak the shaker in hot water for a
    while to dissolve what's left inside. Then because the silly things
    are shaped so you really can't get a grip on them, use a couple of
    the thin rubber jar opener helpers to try and open it. If that
    doesn't work, squirt some LPS - from any ACE hardware store on the
    seam that screws together to loosen it.

    If all else fails, drill a hole in the bottom, and use a rubber plug
    to fill and empty the shaker. And don't leave salt in it. You will
    need to make a jig to hold it to drill, again the bullet shape is
    hopeless to grip.

Judy Hoch

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project