========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     A friend of mine recently found an old silver coin (1697) with a
>     lump of what looks to be rust embedded on the face of the coin.
>     He's tried all sorts of things to get the lump off, but with no
>     success. Anyone have suggestions? 

    Now bear in mind, one might not like what you find underneath once
    the corrosion is removed....may have a patch of pitting underneath... 

    Might try soaking it in household ammonia.....I recently cleaned up
    a silver jital that way..... Time is anywhere from a few hours to a
    week, depending.... The solution might turn blue....so use a tongs or
    something to take the coin in and out....Used a small glass bowl for
    this... 

    If that doesn't do it, you can try alternating with the ammonia and
    vinegar or lemon juice....cleaning with soapy water between baths... 

    Good luck to your friend....cleaning patches like that sometimes is
    like a crap shoot... 

Gary W. Bourbonais
A.J.P. (GIA)

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project