From: Beth Thompson Date: Thu Nov 10 21:52:34 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Daniel > Pure palladium is unsuitable for most common jewelry uses. Too > soft. I have spent quite a few hours working and developing > variations of 950Pd. I would like to understand whay you say it is too soft. I made chain links 12mm in diameter using.999 palladium and the only problem I had was having to reheat the wire I made after pulling it through the draw plate once it doubled in length. I waxed the wire each time before pulling it... I wasn't so much sticky as brittle and when I noticed this I then just reheated it. Are you refering to casting palladium? How is your variation different and is it whiter than fine palladium, Beth Thompson Cimmaran Designs Edinboro, PA ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project