Hi Natalie,

    Have you considered any of the water torches? As long as you're not
    doing reticulation (or other work that requires oxidation), and if
    you don't need to do large scale melting (for casting, for example),
    you might want to look into one of these, since they don't require
    the storage of *any* gases -- they convert distilled water and
    denatured alcohol into hydrogen and oxygen on demand -- and are
    specifically approved for use in residential areas and malls.
    Although they're considerably more expensive that simple gas torches
    (i.e. USD$1,000-4,000 range), and have significantly smaller
    diameter, hotter flames, which take a little adjustment to get used
    to, there are several; models out there that'd do the trick for you.
    Chances are, if I've thought to write to you, so will several of
    their manufacturers. If not, look at the Hydroflux Welder and Elma
    torches in the current Rio Grande or Stuller tool catalogs. (And no,
    I'm not affilliated with them , although my money sometimes is.) 

Good luck,
Doug

Douglas Turet, G.J.,
Turet Design P.O. Box 242
Avon, MA 02322-0242
Tel: (508) 586-5690
Fax: (508) 586-5677
doug. at .turetdesign.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project