========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Zoe, soldering copper requires lots of flux. Try using white paste flux. Torch control is also necessary, to heat the entire piece to flow temp of your solder. Try fluxing the hell out of the piece, cut pieces of solder to sit inside the bezel touching the bezel as well as the back and heat the thing from underneath with large gentle flame. You can pick the edge of the piece up with a poker made of a wire hanger and get the flame under the piece. I usually pick the edge up after the flux has boiled and I am sure the bezel in in the correct spot, the flux will hold the piece in place so it won't slide off as long as you don't pick it up at too much of an angle, angle the torch under the piece rather than the piece over the torch. Your solder surface is also important, I use the honey comb ceramic blocks and can also bounce the flame off them up onto the back of the piece as I lift with the poker. The soldering surface can be a real heat sink and can inhibit solder flow if not very reflective like the honey comb material. Write if you have any more questions; pataniajewelry AT earthlink.net Sam Patania, Tucson www.patanias.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project