    Mical, I had a job over 30 years ago at a silver repair shop in
    Chicago. I removed and replaced knife blades there, and if I remember
    correctly, they are easily removable with a little heat. The filler
    inside the handle is a sort of resin or something, and it softens
    with heat. Also, the connection was finished with a little tin solder
    at the point where the blade meets the handle, so you must heat there
    to about 400 F to melt that solder. You may find that this is not all
    too difficult. It is not too risky, either, because of the low heat
    required. Once you get the blade in place again, tin solder it to the
    handle, wiping off any excess tin while it is hot, with a rag. Then
    scrape off any excess that remains, until it is only in the joint and
    not on the surface nearby. Then polish to remove any tool marks you
    may have left in the area. Good luck! I think you can try it! 

M'lou Brubaker, Jeweler
Goodland, MN
www.craftswomen.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project