>      So, did my expensive purchase solve the "blooming" of boric acid
>     crystals? Nope 

    Here are a few suggestions that may help to control the growing
    crystal of borax that decorates the lid of the alcohol/borax
    container. 

    I mix small amounts of the solution, and freshen it up as needed.  I
    use smaller amounts of borax, so the solution is not too thick, and
    repeat the application several times to build up several thinner
    layers which seem to coat the piece better anyway. (My solutions are
    saturated, but without too much excess laying on the bottom of the
    jar.) When I get ready to solder, I take a few seconds to knock some
    of the residue from the top back into the jar, (since I do it
    regularly, it's a relatively thin layer) and remix it into the
    solution. I also wash out the top of the container periodically,
    since it's the inside lip of the cover which tends to build up some
    crystallization, and keeps the seal from being tight. Lids that have
    a thicker plastic seal work better than those that don't. Hope this
    helps. 

Melissa Veres, Engraver
mveres AT fast.net

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project