>>     Remember that Argentium melts at a lower temperature than
>>     traditional sterling. AFIK, you can only use easy solder with it
>>     anyway. 

>         Just because argentium sterling melts at a lower temp than
>     regular sterling doesn't mean that you still don't need hard,
>     medium and easy. Other suppliers provides all three grades of
>     argentium solder.

    Actually I corrected myself in another posting.  Regular sterling
    solders in extra easy, easy, and medium grades were recommended for
    use with Argentium.

    The new Argentium solders in "easy", "medium", and "hard" do not
    correspond to the same named grades in traditional sterling solders -
    the melt/flow temps are lower for the Argentium, so that each grade
    of Argentium solder is approximately equivalent to the next grade up
    in traditional sterling solder (eg AS easy approx. Sterling
    extra-easy). 

Sojourner

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project