    I make a lot of chainmaille and cut thousands of sterling jump rings
    at a time (I use Pro-Cut on the coils) and the easiest way I have
    found to remove the waxy build up is with a quick dip in an
    amonia/water mixture. 

    I mix 2-3 cups water and add 1/2 cup amonia (from local gorcier) to
    the water. I place the freshly cut rings in a small mesh strainer and
    a quick dunk and swish with the fingertips (30 seconds or so) takes
    the wax (Pro-Cut) off w/o any problems.  

    Remember to rinse the rings when done, the amonia will patina the
    rings if it is left on for too long. 

    If you do this in your sink, don't lean over the basin as you clean.
    The amonia will burn your eyes and nose. And, when rinsing, don't
    loose any down the drain as disposals don't really like jump rings.
    :-) 

    I keep my "cleaner" in a small resealable tub and it is good for
    months. The solution will turn blue with time, as the sterling "dust"
    (left from cutting) gathers and patinas in the solution. 

    I have also use Simple Green in a pinch, and it works just fine, but
    it takes a little longer to clean the wax. Plus, there are no
    chemical issues to deal with. 

    Feel free to contact me offline with any other ring production
    issues or questions. 

Jeff

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project