Re: [Orchid] Argentium Experimentation  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: Karen Tremblay
Date: Fri Aug 05 21:43:04 2005
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    Okay, so I'm understanding that in order to activate the tarnish
    resistance of the Argentium I'll need to heat treat the finished
    product. I'm curious as to how this will work for those of us who
    love to combine silver wire with freshwater pearls in the form of
    chain, knitting or wire wrapping? Won't the heat of the precipitation
    hardening damage the pearls? 

Karen Tremblay
KaeLynn Jewelry Design
Timmins, ON
(705) 360-5861
www.KaeLynnDesign.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project