From: Ladysmithgallery Date: Thu Aug 04 22:38:44 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Trevor, Try to have a little more patience with us argentium newbies. You and Cinthia Eid are two shining lights in our argentium world - you've paved the road for the rest of us, and we are grateful. What you are reading here is the normal learning curve for any new product. And because metal is the heart and soul of what we do, when a new alloy hits the market, there are bound to be bugs that have to be worked out. What we need is correct information to get the most out of the material - this would be true for anything, not just argentium silver. Most of us hadn't heard about the need to raise the germanium to get the best results, and when argentium started to be sold widely, you started to hear about some problems. When you say that everyone should assume the argentium they buy has not been treated, you are speaking from the perspective of a metalsmith. What about the wire wrappers who have never touched a torch? I see this as a problem - one that could be rectified if the suppliers would sell it "ready to use". I have just bought a bunch of argentium sterling, and plan to use is almost exclusively, and I am prepared to anneal! So take a deep breath, Trevor, we all want to love argentium as much as you do! We just need the facts. Keep up the good work, Donna SilverSorceress Designs Unique, handcrafted Silver and Gemstone Jewelry http://www.silversorceress.com/ ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project