From: Trevor F Date: Thu Aug 04 22:37:34 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > Remember that Argentium melts at a lower temperature than > traditional sterling. AFIK, you can only use easy solder with it > anyway. Stuller's "Metals" book, for example, lists the following: Traditional sterling: - melt 1640 F / 893 C - flow 1750 F / 954 F Argentium Sterling: - melt 1410 F / 766 C - flow 1610 F / 877 C Stuller offers Argentium Sterling (AS) solder in three grades: Hard, Medium, Easy. Each has melt and flow temps slightly less than the corresponding grade of regular sterling silver solder. All three grades of AS solder are perfectly usable. There is no known or reported reason why "you can only use easy solder". Cheers, Trevor F. in The City of Light www.touchmetal.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project