Michael,

    I would suggest that you invest in an ionic cleaner. I have been
    using one since September, 2004. I no longer use my ultrasonic at
    all. 

    The ionic cleaner is safe for all stones, including opal and pearls.
    There are no harsh chemicals and no offensive odors. It is also
    totally quiet (unless you have the turbo model and turn on the turbo
    for heavily soiled items like metal expansion watch bands). The
    solution lasts almost forever and the cleaning time is about 45
    seconds. 

    Only one caveat: Silver can somehow cross-contaminate itself if two
    parts of an object are touching each other. I have found that I
    usually get great results with silver by just swishing it around in
    the solution for about 10 seconds with the power OFF.

    After taking the item from the ionic cleaner I rinse it thoroughly
    in running water, dry it with a hair dryer, and give it a final touch
    using a good cleaning cloth such as Fabulustre or Stuller's Ultra
    cloth. 

    Del Pearson of Designs of Eagle Creek in Beautiful South Texas

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project