>         I have made a series of shape cutters for sterling sheet. But
>     having put the sheet in place, between the positive and negative
>     dies, I'd never give it a bash! My method is to put it in a bench
>     vice, tighten to grip it, then tighten fully with a swift turn of
>     the handle, and that gives a nice clean cut without spoiling the
>     dies. 

Hi John and Kim,

    I was reading this line and like the vice idea to punch shapes. This
    just a thought. If you had a spare heavy duty vice laying about and
    say support beam or a barn beam. You could mount the vice
    vertically! Either close the vice up or down. To your taste which
    way. That way you could sit the die and punch on one jaw and then
    just tighten down. Without having to hold the die with one hand and
    tightening with the other. 

    Just a suggestion for the college guys that usually doesn't have a
    big tool budget. 

Jim Zimmerman
Alpine Custom Jewellers & Repair
http://www.handengravingcanada.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project