Reev,

    Un-soldering is a skill as well as soldering.  If you have already
    pickled the piece, and before adding any flux, I protect the other
    joins  with an anti flux and let it dry.  For the anti flux I prefer
    Stop Flow, it will not allow the solder to flow. Then I add the
    SLIGHTEST amount of paste flux to the join that I wish to separate,
    just enough to be where the  solder has attached one piece to
    another. I then use the powers of  gravity. I hold the piece by the
    bail with a heat proof tweezers. I apply the heat gently and directly
    to the join at the bottom of the bail and when the solder melts, the
    weight of the piece will make the piece drop off  the bail. You do
    have to account for the "drop" and make sure the piece will not go
    too far and get damaged.  This is much easier to do in gold,  but
    will work just fine in silver; remember with silver that you may have
    to  bring most of the metal to temperature even if you are
    un-soldering. Its a fine  line between melting and un soldering. 

Beth Katz
http://www.myuniquesolutions.com
Paste Solder and Powder Solder for Jewelers and  Metalsmiths

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project