========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > ... I once solved this problem by using two identical hammers and > putting one in a vise to use as the "anvil". Very tedious trying > to keep the hammers centered. I think making a device incorporating > two domed surfaces and a long u shaped connecting piece to keep > them aligned mi The two hammer suggestions gave me an idea. A simple rack type arbor press ( cheap) or maybe better- a screw (flypress) press ( relatively expensive) could be set up with identical dies top and bottom. This would allow identical impressions ( coining) on both sides. The Flypress would be better. http://www.oldworldanvils.com/flypresses/index.html I have a baby size 0 -- someday I will try it for this.== making some dies tonight. The flypress will be easier to control a reproducible depth of the impressions.Either tool would go pretty fast. jesse ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project