From: jlh/nlh Date: Wed Jul 13 20:57:59 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Keneth, Advise your client that at no time should she (or he) subject gold to bleach (chlorine) at any time for whatever purpose. That includes swimming pools with chlorine disinfectant, washing clothes, etc. Chlorine attacks gold alloys and causes a condition called Chloride stress corrosion. This results in weakening of the metal and eventual breakage and is the cause of many lost stones. As for the green cast,I don't know. Doesn't sound too good. I would try sanding and repolishing but wouldn't have much faith in the remaining strength of the metal. Jerry in Kodiak ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project