========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== For what it's worth, I never ever pickle after enameling. It always etches the enamels (even the blues - all colors, all leaded), and even the mildest etch ruins the beautiful enamel sheen. Since I also use silver, the cleanup is not difficult. First, I cover the enameled area with blue painter's tape. It adheres well but never damages the surface. Then use a mild abrasive like a 3m radial disc brush in a fine grit or possibly a pumice wheel. If you feel pickle is absolutely necessary, use the painters tape then apply pickle with a paintbrush only to the silver areas & rinse within 15-30 seconds; reapplying as necessary. Tarnex can also work in this way. It's extremely difficult to fix the etch - it clouds over if re-fired and is very difficult to polish out. I'd avoid it at all cost. Good luck! ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project