    Hello Ron, I've been out of pocket for quite a while and am catching
    up on all the Orchid postings. 

    I mounted a whole elk tooth as a watch fob.  My customer did not
    want the root cut off, so I made a sort of cone in 18K that closely
    fit and concealed the root.  The cone was textured to resemble tree
    bark, and gold wire and leaves were soldered to the bark in
    vine-like fashion.  The ivory of the tooth was exposed at the end of
    the cone.  As the tooth root is hollow, I drilled into it from the
    root tip (phew), filled the cavity with epoxy, and  screwed in a
    bail with a spiraled end - rather like an eye bolt.  When the epoxy
    set up, the spiral was secured inside the root, with the bail above
    the small end of the cone. 

    I think cutting off the root would have made the project MUCH
    simpler - just like setting a cab then.  Let us know how you
    complete your elk tooth project. Judy in Kansas

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project