    Thanks for the idea Wayne. Because I was about to take a class on
    designing with briolettes, I recently reviewed all the info on Steve
    Green's site and noted that, rather than the usually bead-style
    horizontal drilling, which he says weakens the stone, he recommends
    drilling straight into the top of a briolette and using a "pearl
    post" (or better, a cap-post) with Devon 2-Ton Epoxy.) I never
    thought of using the same technique for end balls, but why not? 

    By the way, the briolette class covered various methods of wire-
    wrapping, and I don't think the instructor would have smiled on the 
    use of adhesive. (Unfortunately, I can barely afford the "weak" 
    briolettes, never mind Steve's gorgeous stones.) Then, Friday, when
    I  went to the opening for the MAG show, I saw a necklace made by 
    someone who may have devised her own briolette technique. The 
    necklace was a joke (literally--after all, this was a "metal arts" 
    show), but she'd made triangular wire elements, with the middle of 
    the base missing, and glued the ends into the horizontal drill
    holes.  The technique doesn't allow the briolette itself to
    move--which was  something my teacher's techniques emphasized--but
    it might strengthen  them. And it looked good, too. 

    Lisa Orlando Aphrodite's Ornaments 

    PS: If you can see this show, do--a Beth Rosengard brooch and John 
    Jenkin's exquisite and terrifying Icarus knife make it worth the 
    trip. (Well, there's also a Kent Raible ring, but he doesn't post 
    here... ) 

    http://www.ganoksin.com/orchid/archive/200506/msg01278.htm 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project