Lisa

    Propane and butane are both naturally occurring hydrocarbon
    compounds that are components of natural gas.  When they are burned
    efficiently (such as in a soldering torch)  they both form carbon
    dioxide and water as by-products. MAPP gas is also a hydrocarbon and
    also forms carbon dioxide and water when burned.  Since all three
    produce the same gasses once they are burned, I don't believe that
    one can be considered more ozone friendly than the other. 

    The amount of any one of these gases that you would burn in your
    torch in a year is minute, compared to the amount of similar
    hydrocarbons that are burned in a year in say your furnace, your
    home water heater, your car, in making electricity to run your home
    etc.  You can do far more for the ozone layer by lowering your
    thermostat in the winter or raising it during air conditioning
    season, or by leaving your car at home and taking public
    transportation or riding a bike. 

    My suggestion is that you buy the best torch for the job and
    consider other ways to conserve energy use and thus reduce your
    impact on the ozone layer. 

Regards
Milt Fischbein - Jewellery Artist
Calgary AB, Canada
www.members.shaw.ca/a925maven
a925maven AT shaw.ca

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project