    I don't know whether my solution to this problem will appeal to
    others, but here it is-- 

    Rather than deal with paste solder vagaries, I bought powdered
    solders. I dip my solder pick into paste flux, then into powdered
    solder, then place it where I want it. I am very happy with this
    system. The paste solder I have doesn't always want to stick where I
    put it, and it smokes when heated. The little "worm" of solder tends
    to curl up over the needle as I extrude it. I like the powder much
    better. I can pick up pretty much the exact amount I need, so
    there's no question of what to do with extra that oozed out of the
    tube and is tough to put back. 

    You kmow, I think I'll write my next column for the CMAG newsletter
    about powdered solder! By the way, I bought the powdered solders from
    our own Beth Katz, (Unique Solutions:
    http://www.myuniquesolutions.com) when I was at SNAG last year. 

--Noel


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project