From: Cynthia Eid Date: Wed Jun 01 23:43:01 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > To anyone using Pripps, I'm working on a large sterling cup and > I've been through something like 5 hardware store spray bottles > (for spraying Pripps). They just quit working-- no spray. Some > clog, but most just simply won't produce any liquid no matter how > many times I squeeze the trigger (which squeezes freely and > smoothly). Hi Andy, I haven't used Prip's for a while in my own work, since discovering Argentium Sterling. However, I definitely am familiar with the problem you describe. Try using a "I Can't Believe It's Not Butter" spray bottle (can you tell that we have a cholesterol problem in our family?!) Also, I like (well, used to like) the spray bottles sold at CVS, etc. for travel uses. With either one, try keeping a container of water on hand, and put the sprayer upside down in the water, so that it cannot dry up in the nozzle. Another thing you can do when the spraying thing really gets on your nerves: * put the Prip's in a wide-mouthed jar or container. * Get a wide, cheap paint brush. * Dip the brush into the jar of flux, and brush it on, much as you would spray---That is, brush a bit of flux onto the sterling. Heat the metal until the flux turns to white powder. At that point, start alternating between heating and brushing the flux on, just as you would alternate between heating and spraying, until the metal is covered with white powder. * (keep the brush very wet, so that you don't fry any bristles. It really does not matter much if you do , though. You used a cheap brush, right?) I hope this helps! Cindy www.cynthiaeid.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project