    My solder area is outside. In the summer time it gets above  100
    degrees during the day. I have had one sprayer that has worked for
    several years in both summer and winter. I do not keep the sprayer
    capped. It sits on my outside bench all the time. I am wondering if
    there is something different about the consistency of pripps flux.  

    This is not meant to be a sales pitch for Cupronil but that is  what
    I use without getting a clogged sprayer.  

    We have had trouble getting the chemicals in Cupronil to completely
    dissolve in some tap waters.  I am no chemist but I assume the
    hardness of the water may have some affect on the ability to
    completely dissolve  the chemicals.  We use distilled water as a
    carrying agent. You might  want to try using distilled water. 

    We buy our sprayers from a plastic bottle distributor in  Phoenix. 

    Using a brush to apply anti fire scale flux is the original  way it
    was applied. Heat the metal until the flux paints on like whitewash.
    Too hot and the brush sticks or burns. To cold and the coating
    washes away. Painting it on is somewhat time consuming.   

    It is very late here and I find I can't sleep.  I  have to retype
    about every third word. I guess that is a measure of  how tired I am
    getting. 

My 2 cents worth.
Lee Epperson

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project