Hi Vicki,

    Many years ago, I did a line of found object jewelry and had a whole
    collection of guitar string jewelry. A few suggestions from what I
    learned about the material. 

    You can wrap the strings into little 'wreaths' around a mandrel 50%
    smaller than you want the finished circumference to be as the core
    of the string is very very springy. Use these little bundles for
    earring parts, necklace links or parts or pins. I did not have much
    luck with bracelets because the coiled strings really tweak arm hair
    and are not very comfortable. 

    I secured the ends of the 'wreaths' by doing a noose-type knot with
    22ga fine silver wire. The coiled material of the string can also be
    unwound to expose the core and then a bead can be threaded on. Secure
    the end by bending it into a tight jump or laser weld a beaded end to
    secure. 

    After the piece is finished, ultra sonic and magnetic tumble for a
    beautiful soft finish. 

    We tried sourcing the old strings of a few high profile rockers with
    not much luck....what an awesome appeal a line like this would have!

T Lee
T Lee Fine Designer Jewelry
18 University Ave NE
Minneapolis, MN  55413
(612) 789-2656
(612) 677-3700 fax
www.tleegold.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project