Re: [Orchid] Argentium Blog  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: Zen Sojourner
Date: Thu May 12 19:57:12 2005
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>    Try Hauser & Miller
>    http://www.ganoksin.com/resources/detail-hauser_and_miller-1616.html
>    in St Louis. 

    In St. Louis, huh?  That's almost my neck of the woods. 

    The problem with drawing it down is that my use for the finer wire
    is for crochet, and I like loooooong pieces for that.  There are ways
    to work in a new strand, but its a pain (at least it is for me while
    I'm still learning). 

    I thought Stuller was currently the only US supplier of Argentium? 
    I went to the Hauser and Miller website and couldn't find a mention
    of Argentium. 

    Not doubting you, just can't find it on the website. 

Sojourner

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project