========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Here in the UK the rule has been that metals are only hallmarked to the value of the lower grade metal unless the higher grade metal part is easily and completely detachable. While I appreciate that hallmarking regulations in the US are not as rigorous as in the UK, I would have thought that common sense would suggest that, unless the two metals are in almost equal proportions, the standard of the larger proportion should take precedence. For example, would you advertise a silver ring with a couple of inlaid gold stars on the table as a 'silver ring with gold decoration' or a 'gold ring with a silver shank'?? Unless the standard mark is put onto the actual metal that it refers to (such as the gold stars in the above example) it could easily be construed as misleading. For example, in this ring, would both gold and silver marks on this ring shank mean that the shank was gold and silver plated or that it was made of a combination of silver and white gold or maybe its a white gold ring with silver stars which have been oxidised to a nice golden hue??? Best Wishes Ian Ian W. Wright Sheffield UK ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project