========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I just read your posting on trying to etch silver plate over nickel. Your solution is probably too strong to be the most effective. You need to get your solution down to 10%-30% strength. Use distilled water, not tap water; acid into water. Now then, to rain on your parade--no one who hasn't had *chemical hazard* training and access to a fully equipped lab setting, with an eye wash station and dump shower, should be using the highly caustic acids. There is just too much potential for a serious accident, particularly with your lung tissue. Please consider using a safer alternative, such as ferric nitrate. It has a slower etch, yes, but the nice advantage is that it will stop when it gets to the nickel. Useful for multiple metal laminations, say when you want a contrast situation, or to remove some material in mokume, so there is more relief contrast. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project