From: Bruce Holmgrain
Date: Sat May 07 20:17:11 2005
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>        I am getting ready to do a project using a blend of Pure
>     Silver, Palladium, Ruthenium,Platinum, and will be using
>     Hydrogen/Oxy from the torch to do the melt and pour and I will use
>     an Argon Gas to put a blanket of inert gas over the melt to keep
>     down the scale and carbon. 

    Although I have never tried this particular combination, I have
    never found oxides of either palladium nor ruthenium to be a
    problem. I have only used ruthenium sponge to make 95% platinum
    alloy. Oxides have never been a problem for that. Palladium gives up
    it's oxides at around 1100F. Silver only oxidizes in ozone. Even if
    oxygen was to be a problem, I am puzzled as to how you would "cover"
    your melt with argon when a high pressure stream of burning gas is
    blowing it right off of the melt. What percentages are you
    considering? Perhaps the the silver and platinum will cover the melt
    just fine? 

>        I will be soldering pieces of 22K Green Gold on the cast pieces
>     an will I need to go back to Butane/Oxy to do that? 

    Just about any torch will do on this soldering job. 

Bruce D. Holmgrain
Goldwerx
http://www.goldwerx.com
guy AT goldwerx.com
JA Certified Master Benchjeweler, CAD/CAM Services

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project