>         I am getting ready to do a project using a blend of Pure
>     Silver, Palladium, Ruthenium,Platinum, and will be using
>     Hydrogen/Oxy from the torch to do the melt and pour and I will use
>     an Argon Gas to put a blanket of inert gas over the melt to keep
>     down the scale and carbon. 

    Palladium really likes to absorb hydrogen, you will likely cause
    yourself some porosity problems if there is a significant amount of
    palladium present. Use oxy/propane it will melt all the above metals
    without too much problem from a gas absorption standpoint. How do
    you plan to apply / keep the argon over the melt if you are torch
    melting? 

>         I will be soldering pieces of 22K Green Gold on the cast
>     pieces an will I need to go back to Butane/Oxy to do that? 

Jim Binnion

James Binnion Metal Arts
Phone (360) 756-6550
Toll Free (877) 408 7287
Fax (360) 756-2160
http://www.mokume-gane.com
jbin AT mokume-gane.com
Member of the Better Business Bureau

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project